    I try to clarify the numbers a little (ok I'm...

    I try to clarify the numbers a little (ok I'm European and I don't use thumbs). in physics it is used to put the comma (or the dot) only as a function of the precision of the measurement of the...
  2. Replies
    4
    Views
    359

    ARs have been my daily bread for 30 years (of...

    ARs have been my daily bread for 30 years (of which 10 as a process engineer for the world's leading manufacturer of AR implants), let's see if I can clarify a few things:
    1 measuring the thickness...
  3. usually the lenses that have a spin coating...

    usually the lenses that have a spin coating treatment have the CX side already hardened with a non-colorable HC, so +/- all the spin coater uses non-colorable HC. It is not possible to color the lens...
  4. Replies
    3
    Views
    3,355

    1 these are only products that are used to clean...

    1 these are only products that are used to clean the lenses, they have no effect on hardness, of course if you use lenses with a protective coating on cx, this will be affected and / or removed.
    2...
  5. Replies
    7
    Views
    679

    sorry but I got confused, capture 2 is with the...

    sorry but I got confused, capture 2 is with the ZrO2 and capture 3 is just Cr39 + top coat
  6. Replies
    7
    Views
    679

    1496114962

    1496114962
  7. Replies
    7
    Views
    679

    sorry but I did not understand, to really measure...

    sorry but I did not understand, to really measure the thickness you would have to evaporate a very high thickness (at least 1/4 lambda), if we suppose the refractive index around 1.31 means at least...
  8. Replies
    7
    Views
    679

    14960

    14960
  9. Replies
    7
    Views
    679

    14959

    14959
  10. Replies
    2
    Views
    487

    we have used deep coating systems with tintable...

    we have used deep coating systems with tintable hard coat + primer for many years, they also work on poly but in recent years we have completely abandoned poly in favor of Trivex and 1.6 (colored and...
  11. Replies
    71
    Views
    13,528

    in my continuous laboratory with the traditional...

    in my continuous laboratory with the traditional Bayer test (I am well stocked with Alundum) I would like to know the specifics of the sand used for the Essilor test
    quartz microspheres...
  12. Replies
    26
    Views
    66,520

    846 / 5000 Risultati della...

    846 / 5000







    Risultati della traduzioneWe produce lenses and treatments for opticians, usually supplying samples in two folders of 24 lenses for free or at a small cost.Usually a folder...
  13. Replies
    17
    Views
    2,234

    you are right, in Italy it is very different and...

    you are right, in Italy it is very different and such an approach would not be accepted. I must deliver a PAL freeform, colored, with hard coat and AR (or mirrow or both CX mirrow and cc AR) in 3 day...
  14. Replies
    17
    Views
    2,234

    there are 2 commercial types of 1.67, l0MR7 which...

    there are 2 commercial types of 1.67, l0MR7 which dyes very quickly but has problems with heat (softening temperature 74 ° c-165 f °) and MR10 which has no problem and you can treat it as CR39 at 93...
  15. Replies
    17
    Views
    2,234

    we use tintable HC (deeping), colored the lens,...

    we use tintable HC (deeping), colored the lens, soft cleaning by ultrasonic tanks (no color change) and AR coat, we send to customer in 2 days.
  16. Replies
    1
    Views
    648

    I'm sorry but the arrangement of an...

    I'm sorry but the arrangement of an anti-reflection process that has between 4 and 10 layers is a complex thing, firstly you need a spectrophotometer to evaluate the reflection curve and secondly a...
  17. please post a photo, the lenses with these...

    please post a photo, the lenses with these problems are only HC hardened? with what products do you raise them? is the phenomenon only concave or also convex?
  18. Replies
    2
    Views
    4,394

    the first step is to visually determine whether...

    the first step is to visually determine whether the gap is between HC and lens or between HC and AR.
    If HC also delaminates, try HC only lenses in boiling DI water for 15 and after 15 extra minutes....
  19. UK is no longer an EU country as of January 1st....

    UK is no longer an EU country as of January 1st. Now they cannot even be the country of entry for CE marking
  20. Replies
    21
    Views
    5,364

    14786

    14786
  21. Replies
    21
    Views
    5,364

    14785

    14785
  22. Replies
    21
    Views
    5,364

    second...

    second
    https://www.optiboard.com/forums/image/png;base64,iVBORw0KGgoAAAANSUhEUgAAApUAAAE1CAYAAAC2pRvUAAAgAElEQVR4Ae3d7cscx7nn8f675k8I 8IEwsKKJcmb5nDWL3YNy3pfxDmSE92JziIGb2IWQRCH...
  23. Replies
    21
    Views
    5,364

    these are the measured transmissions of a CR39...

    these are the measured transmissions of a CR39 lens and the same lens with an AR on both faces.
    The transmission increases and a lot
    Shimtzu UV2600 spectrophotometer instrument with integrating...
  24. Replies
    20
    Views
    5,089

    I use a tintable HC on MR8 and MR10 with good...

    I use a tintable HC on MR8 and MR10 with good results, which HC would you like to use? you also want to use Primer (it helps a lot in the color speed )?
  25. Replies
    16
    Views
    2,873

    top coats based on PFA or PTFE normally resist...

    top coats based on PFA or PTFE normally resist almost all chemicals (but not wear and tear), silicone top coats have a lower seal and are removed by continuous washing with solvents